Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SDETERS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Post tension concrete flat plate with irregular column spacing

Status
Not open for further replies.

oranda

Civil/Environmental
Oct 24, 2001
21
When designing post tensioned concrete flat plate with irregular column spacing (ie. when one column strip in one span intersects another column strip of another span running perpendicular and the columns in both direction don't line up), would you consider the effect of any concentrated forces from one column strip on another column strip it's intersecting?

Would you also know any articles or reports from magazine and journals which may be related to this topic?
 
Replies continue below

Recommended for you

Please read section 5.3.8 in

Post-Tensioning Manual
5th Editon
Post Tensioning Institute

in which the method of balancing loads is put to good use for plates with irregular layouts.
 