quizzical1
Mechanical
Hi All,
Just wondering if I could get a few suggestions as to the best coating to reduce / avoid sticking for a 303 SS spool valve (can be another metal if need be).
It will be used in hot/cold water mixing with temps ranging from 45F - 70F cold side and 100F - 150F hot side if this matters.
Can anyone recommend a preferred coating to minimize scale build up while not wearing off during operation?
Thanks,
Glenn
Just wondering if I could get a few suggestions as to the best coating to reduce / avoid sticking for a 303 SS spool valve (can be another metal if need be).
It will be used in hot/cold water mixing with temps ranging from 45F - 70F cold side and 100F - 150F hot side if this matters.
Can anyone recommend a preferred coating to minimize scale build up while not wearing off during operation?
Thanks,
Glenn