Hi everyone.
When I supply pWPS to Contractor for review. He write comment in my pWPS that : due to hardness consideration Contractor advise to use an E 8016 - XX electrode instead of E 9016-G. I don't know why. Hereafter is parameter of pWPS:
+Base metal API 5L X65
+Process GTAW+SMAW
+Root: A5.28 ER80S-G
+Hot: A5.28 ER80S-G
+Third: A5.5 E 9016-G
+Cap: A5.5 E 9016-G
Could Someone explain to me why?
Thanks.
When I supply pWPS to Contractor for review. He write comment in my pWPS that : due to hardness consideration Contractor advise to use an E 8016 - XX electrode instead of E 9016-G. I don't know why. Hereafter is parameter of pWPS:
+Base metal API 5L X65
+Process GTAW+SMAW
+Root: A5.28 ER80S-G
+Hot: A5.28 ER80S-G
+Third: A5.5 E 9016-G
+Cap: A5.5 E 9016-G
Could Someone explain to me why?