Want to know if anyone can direct me to the material properties of A380 die cast aluminum at elevated temps. Particually up to 300C
 
Replies continue below

Recommended for you

ASM Handbook Volume 2 Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, in the chapter titled Properties of Cast Aluminum Alloys.
 
The Kaiser aluminum casting book shows a tensile of 6,000psi and yield of 4,000psi at 600F. Elongation is 45%. These are "typical values".
 