ramakant
Mechanical
- Aug 27, 2001
- 12
i have an equipment where i have to use rubber as gasket.
inside atmosphere is nitric acid fumes. and temperature is ambient and vacuum of 2 m water column is maintained in side.
my problem is that i have to calcutate bolt loads required to get a prefect seal. please suggest me the type of rubber i can use.
will nitrile rubber do? The gasket has to be in position for more than 5 years.
if some body can help me in getting the properties of rubbers (shore hardness 'A' from 5 to 75) i.e. percent compression vs stress generated in...
Thanks and regards
Ramakant
inside atmosphere is nitric acid fumes. and temperature is ambient and vacuum of 2 m water column is maintained in side.
my problem is that i have to calcutate bolt loads required to get a prefect seal. please suggest me the type of rubber i can use.
will nitrile rubber do? The gasket has to be in position for more than 5 years.
if some body can help me in getting the properties of rubbers (shore hardness 'A' from 5 to 75) i.e. percent compression vs stress generated in...
Thanks and regards
Ramakant