ATUL KHATRI
Mechanical
Hydrogen Service
ASME 31.3 gives exemption from PWHT for P.No 1 (carbon steel piping material) irrespective of thickness with a clause of Preheating above 25mm nominal thickness . So still "carbon steel with PWHT" curve shall be applicable as per API RP 941 ?
If yes than will there be any governing thickness for the same?
Wet Sour Service
Requirement of PWHT for SSC (Sulfide stress cracking) and associated crackings HIC,SOHIC is not clearly mentioned in NACE MR0103 for piping material. What should be the criteria for the same ? Though MR0175 does exempt the requirement of PWHT if CS, LAS comply the hardness requirement as mentioned in Table A.1 of MR0175.Please clarify
ASME 31.3 gives exemption from PWHT for P.No 1 (carbon steel piping material) irrespective of thickness with a clause of Preheating above 25mm nominal thickness . So still "carbon steel with PWHT" curve shall be applicable as per API RP 941 ?
If yes than will there be any governing thickness for the same?
Wet Sour Service
Requirement of PWHT for SSC (Sulfide stress cracking) and associated crackings HIC,SOHIC is not clearly mentioned in NACE MR0103 for piping material. What should be the criteria for the same ? Though MR0175 does exempt the requirement of PWHT if CS, LAS comply the hardness requirement as mentioned in Table A.1 of MR0175.Please clarify