1973Patrick
Petroleum
- Aug 6, 2012
- 14
Hi,
What is de T range if:
SMAW - Plate 15 mm - V-groove - P6 - PWHT and Impact tested in PQR
Table QW-451.1 ASME IX said: Over 3/8 (10), but less than 3/4 (19) = 2T for T for base metal.
Someone told me that T = 1.1 x T because Impact test and PWHT performed during the PQR
Is that so and where is this described in te ASME IX?
Thnx!
Patrick
What is de T range if:
SMAW - Plate 15 mm - V-groove - P6 - PWHT and Impact tested in PQR
Table QW-451.1 ASME IX said: Over 3/8 (10), but less than 3/4 (19) = 2T for T for base metal.
Someone told me that T = 1.1 x T because Impact test and PWHT performed during the PQR
Is that so and where is this described in te ASME IX?
Thnx!
Patrick