zakk
Mechanical
- May 3, 2002
- 48
We have forgings supplied in accordance with ASME SA350-LF2 Class 1 in the Normalized condition (P1 Group 2). The hardness came in between 130 and 140 HBN, which is too soft for our application (galling issues). We segregated a portion of the material to which we applied a quench and temper and got the hardness up to 170 to 180 HBN and reduced our galling issues.
Does ASME Section VIII Div 1 permit an entity other than the material manufacturer to change the heat treatment condition of material if it is performed per the material specification and supplementary testing (tensile, hardness, charpy, etc.) is documented as meeting the material specification?
Does ASME Section VIII Div 1 permit an entity other than the material manufacturer to change the heat treatment condition of material if it is performed per the material specification and supplementary testing (tensile, hardness, charpy, etc.) is documented as meeting the material specification?