Questions regarding ASTM A90/ A 90M 1

Status
Not open for further replies.

Naruwan

Materials
Jul 19, 2010
46
Hi guys,
according to ASTM A90/ A 90M, nothing was mentioned about the removal of a paint coating before performing the stripping test as to determine the mass of coating on Iron or steel plates with metallic coating. Is paint removal a good media to remove the paint without jeopardizing the mass of the metallic coating?

Thanks!
 
Replies continue below

Recommended for you

Yes, provided paint removal does not disturb the substrate zinc coating.
 