If 6 mm P.No.8 material is welded with 38 mm P.No.1 material, what would the thickness range qualified in this case?
QW-202.4 deals with Dissimilar Base Metal Thicknesses, in the question not only base metals are of different thicknesses but also have different P.No's and QW-202.4 gives qualified maximum thickness criteria in a different way for different P.NO's.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
QW-202.4 deals with Dissimilar Base Metal Thicknesses, in the question not only base metals are of different thicknesses but also have different P.No's and QW-202.4 gives qualified maximum thickness criteria in a different way for different P.NO's.