Dec 1, 2018 #1 sftyvlv1 Mechanical Joined Oct 25, 2018 Messages 48 Location CA How would I apply this paragraph to a 6g pipe test? Would I have the welder weld out a new test or root an entire test, fill and cap the section that failed? What should happen?
How would I apply this paragraph to a 6g pipe test? Would I have the welder weld out a new test or root an entire test, fill and cap the section that failed? What should happen?
Dec 2, 2018 #2 DekDee Petroleum Joined Mar 12, 2012 Messages 1,323 Location PH The welder must complete two full 6G test coupons and both must pass mechanical testing. Upvote 0 Downvote
Dec 4, 2018 Thread starter #3 sftyvlv1 Mechanical Joined Oct 25, 2018 Messages 48 Location CA Thanks, much appreciated. Upvote 0 Downvote