SuperStress
Aerospace
- May 5, 2003
- 94
In MMPDS-04 (and previous) the allowable for 7075-T6 bare sheet per QQ-A-250/12 is Fbru=156ksi (0.040"<t<0.125", e/D=2.0, A-basis, Table 3.7.7.0(b1)).
In MMPDS-05 (and on) the allowable is Fbru=146ksi (same parameters, Table 3.7.8.0(b1)). The table says that it was last revised in Apr 2010 per MMPDS-05 Item 09-29.
We are looking at a repair to an older airframe that was designed/substantiated around the MIL-HDBK-5B days, and the margins are low enough that simply replacing the vintage material with new would indicate a negative margin.
I'm trying to find out the reason for this change. My initial impression was that it might be a "wet pin"/"dry pin" reduction, but I can't find anything to back that up, and the reduction seems a bit small for that anyway. I know that there have been reductions on thicker plate materials identified in the tables at the beginning of Ch. 3 (Bearing Property Reductions for Thick Plate of 2000 and 7000 Series Alloys), but I've not seen anything similar for thin sheet.
Does anyone know the history behind this reduction in allowables?
SuperStress
In MMPDS-05 (and on) the allowable is Fbru=146ksi (same parameters, Table 3.7.8.0(b1)). The table says that it was last revised in Apr 2010 per MMPDS-05 Item 09-29.
We are looking at a repair to an older airframe that was designed/substantiated around the MIL-HDBK-5B days, and the margins are low enough that simply replacing the vintage material with new would indicate a negative margin.
I'm trying to find out the reason for this change. My initial impression was that it might be a "wet pin"/"dry pin" reduction, but I can't find anything to back that up, and the reduction seems a bit small for that anyway. I know that there have been reductions on thicker plate materials identified in the tables at the beginning of Ch. 3 (Bearing Property Reductions for Thick Plate of 2000 and 7000 Series Alloys), but I've not seen anything similar for thin sheet.
Does anyone know the history behind this reduction in allowables?