What are practical experiences with refurbishing welded body ball valves for natural gas?
We have some stock of leaking ball valves (PTFE seal, 12", 18", 20", Cooper Cameron, Argus, etc.). Experience with many of new valves (which often comes from China) are worse than 30 years old C.C. or Argus, and we want to save them if possible. We have some vendors which claims that they can refurbish those valves to be useful as new.
How do we ensure this so that we have reliable valve for many upcoming years? Which steps of refurbish steps to control with them, what conditions to set up, how to test refurbished valve? As I know there is API 6DR, and final testing should be as for new valve per API 6D. Is this enough?
1) What is best way to cut valve body?
2) What is best way to weld body back?
(Maybe link to some reference article, video, book, etc...)
3) Is it possible to buy complete original seat packs for old valves as defined or then need to produce some parts from scratch?
4) What are practical experiences with refurbished ball valves?
I hope to get at least some of those questions answered.
Tnx.
We have some stock of leaking ball valves (PTFE seal, 12", 18", 20", Cooper Cameron, Argus, etc.). Experience with many of new valves (which often comes from China) are worse than 30 years old C.C. or Argus, and we want to save them if possible. We have some vendors which claims that they can refurbish those valves to be useful as new.
How do we ensure this so that we have reliable valve for many upcoming years? Which steps of refurbish steps to control with them, what conditions to set up, how to test refurbished valve? As I know there is API 6DR, and final testing should be as for new valve per API 6D. Is this enough?
1) What is best way to cut valve body?
2) What is best way to weld body back?
(Maybe link to some reference article, video, book, etc...)
3) Is it possible to buy complete original seat packs for old valves as defined or then need to produce some parts from scratch?
4) What are practical experiences with refurbished ball valves?
I hope to get at least some of those questions answered.
Tnx.