Dear all,
This is regarding plastic flow simulation using mold flow software.
We have a problem while running analysis with mold inserts,
We tried following two approachs
Approach 1
We meshed mold insert and the plastic part togeher as a single integral part in Meshing software (Hypermesh). Then in MF, we selected appropriate insert surface elements in fusion mesh as mold insert and assigned properties for it .when we fired the analysis in molflow, free edges were indicated after completion of flow,cool analysis and the warpage analysis was failed.The error indicated was free edges along the interface region between insert and plastic area.
Approach 2
In second iteration, By using fusion mesh option,we meshed the plastic volume and meshed seperately the insert volume.now when i check for free edges, Mold flow clearly indicates there are 400 free edges and overlap which is exactly at the interface area.i want to run the full analysis including warp.now the mesh has a good connectivity between both the plastic area and insert area.
We are clueless and look forward for suitable directions to proceed further.
E.Logesh
This is regarding plastic flow simulation using mold flow software.
We have a problem while running analysis with mold inserts,
We tried following two approachs
Approach 1
We meshed mold insert and the plastic part togeher as a single integral part in Meshing software (Hypermesh). Then in MF, we selected appropriate insert surface elements in fusion mesh as mold insert and assigned properties for it .when we fired the analysis in molflow, free edges were indicated after completion of flow,cool analysis and the warpage analysis was failed.The error indicated was free edges along the interface region between insert and plastic area.
Approach 2
In second iteration, By using fusion mesh option,we meshed the plastic volume and meshed seperately the insert volume.now when i check for free edges, Mold flow clearly indicates there are 400 free edges and overlap which is exactly at the interface area.i want to run the full analysis including warp.now the mesh has a good connectivity between both the plastic area and insert area.
We are clueless and look forward for suitable directions to proceed further.