repairing longitudinal weld joint of a high pressure boiler of P no 1 is postweld heat treatment req

Status
Not open for further replies.

stan000

Mechanical
Jul 31, 2014
121

hello friends

Repairing longitudinal weld joint of a high pressure boiler of P no.1 is postweld heat treatment required.

I check PW-39.
STAN

 
Replies continue below

Recommended for you

Follow PW-39 for thickness requirements regarding PWHT for P-No 1 base material.
 