I was wondering if there are any stress relief or other heat treat requirements for hastalloy piping after welding. This is a new material for me. The piping is for chemical service essentially non-corrosive at moderate temperatures.
 
Replies continue below

Recommended for you

No, this material can be left in the as-welded condition.
 
And as you look for info, you be more specific : Hastalloy...B , C ,C4 , C276 ( B in particular is rather different from the others).
 
Sorry. To be more specific Hastalloy c276. Thanks for the insight.
 