The question here is related to a discussion I have had and observed many times over the years.
I'm not interested in what codes/specifications say or do not say, I'm interested in research that shows the results of the "Welds too close" topic that has been addressed here, on jobs, and other places online.
I read through one paper at https://www.researchgate.net/public...uctures_Pipelines_And_Piping_State_Of_The_Art that have me some other references but as someone who is NOT an engineer, this will take some digesting.

I am looking for something definitive that contrasts the difference in mechanical properties resulting from the welds being "too close". I am continuing to look and learn but any information is appreciated that can lead me to the "why and when" separation of welds by a specific distance should be a consideration.

As an inspector, I don't make engineering decisions but this topic has come up many times.

Thanks.

Gerald Austin
Greeneville TN

 
Replies continue below

Recommended for you

It depends.
Regardless of what happens to the material the inspectability is the first question to address.
How are you testing and can you do it properly with very closely spaced welds?
In materials that are very forgiving of welding it has virtually no impact on the properties.
In materials with critical preheat and PWHT criteria then you can mess with things if the HAZs overlap.
 
It depends.
Regardless of what happens to the material the inspectability is the first question to address.
How are you testing and can you do it properly with very closely spaced welds?
In materials that are very forgiving of welding it has virtually no impact on the properties.
In materials with critical preheat and PWHT criteria then you can mess with things if the HAZs overlap.
I have seen the ability to inspect referenced in project documents before. Until the welds overlap, Visual of each joint is possible. RT and offset could definitely be an issue.

I would think that if each joint is welded individually, preheat of each joint is correct. I understand thermal gradients changing with concurrent welding but each individual weld made "properly" is what I am interested in. And you touch on the next thought, if it does "harm" the product, can it be corrected with proper PWHT.

Thanks for the thoughts.
 
Looking at the following Residual Stress Chart with the distance from the weld, it seems that Residual stresses comes down at a distance of approximately 15-18mm. For a Carbon Steel piping normally we take a gap of 50mm between two welds.
1736484998785.png
 
If they are both new welds, made one right after the other and then PWHT I don't have much concern for them being very close.
But when one weld is existing and then another weld is added some time later, I start to worry.
Heat from the weld, overlapping residual stresses, effects of another PWHT can all combine to cause unplanned issues.
One reason that a lot of companies have blanket policies requiring a minimum separation.
 
@pipewelder1999 - there’s a lot more becoming available on open access like the paper I posted. The whole journal is open access which is the best thing because it annoys me greatly when journals that I pay good money to subscribe to then post up some of the content for free.
 