I haven't heard of using Rodine 213 with H2SO4, only with HCL in the range of 0.05%-0.1% v/v.
If we used a Rodine product for H2SO4 it was Rodine 85.
You could contact the Henkel Corp as they took over from Parker who took over from Amchem.