I am working on vessels with 8 barg design pressure @ 670 Deg C and full vacuum @ 670 deg C.
1- When I use SA 240 304H, I get message in material window of Pvelite that "Ultimate tensile strength at external pressure is out of range". The same error is not coming with 304.In table U of ASME sec II, FOR 304H it is not giving any value for UTS AT 550 and onwards. Is there some relationship between UTS at external pressure temperature and Table U?
What does this means can i not use 304H with full vacuum or there is some justification. Kindly explain.
2- Even though client has specified 304, but we are proposing to use 304/304H, so to meet note G12(0.04 % minimum limit on Carbon content) of ASME SEC II. Kindly elaborate our proposal to use 304H and how it should be ordered, i mean as dual grade 304/304H or simply 304H.
3- at 670 allowable stress for SA 240 304 is based on time-dependent properties. what does this means and what further calculation or FEA, buckling analysis we need to do? Design life of vessel s 30 life, with time dependent creep range in consideration do we need to perform any further calculation. I saw somewhere Creep Analysis Using Larsen-Miller Parameter Method and some formulation in API 560 and FSS standard. Kindly clarify what actions or calculation are to be performed to satisfy full design life when in creep range
Thanks
Manj
1- When I use SA 240 304H, I get message in material window of Pvelite that "Ultimate tensile strength at external pressure is out of range". The same error is not coming with 304.In table U of ASME sec II, FOR 304H it is not giving any value for UTS AT 550 and onwards. Is there some relationship between UTS at external pressure temperature and Table U?
What does this means can i not use 304H with full vacuum or there is some justification. Kindly explain.
2- Even though client has specified 304, but we are proposing to use 304/304H, so to meet note G12(0.04 % minimum limit on Carbon content) of ASME SEC II. Kindly elaborate our proposal to use 304H and how it should be ordered, i mean as dual grade 304/304H or simply 304H.
3- at 670 allowable stress for SA 240 304 is based on time-dependent properties. what does this means and what further calculation or FEA, buckling analysis we need to do? Design life of vessel s 30 life, with time dependent creep range in consideration do we need to perform any further calculation. I saw somewhere Creep Analysis Using Larsen-Miller Parameter Method and some formulation in API 560 and FSS standard. Kindly clarify what actions or calculation are to be performed to satisfy full design life when in creep range
Thanks
Manj