Could anyone give me the average thermal conductivity of SA 508 (cl. 2/3) or, better, as a temperature function between 900 and 300 °C?
Thanks a lot
 
Replies continue below

Recommended for you

Here is a tip, review ASME Section II, Part D, Table TCD, and look at Material Groups C and D.
 