IN ASME SEC II, FOR SA516 GR70
YIELD STRENGTH VALUE IS 38000 PSI
AND TENSILE STRENGTH VALUE IS 70000 PSI.
I READ THAT 38000 PSI IS A VALUE FOR 0,2% PLASTIC DEFORMATION
I TRY TO DESIGN A LIFT LUG (ONLY ONE USE AND LEAVE)
AND WANT TO HAVE 45000 PSI STRENGTH VALUE FOR CALCULATIONS.
BUT I WANT TO KNOW THE RATE OF PLASTIC DEFORMATION ON MATERIAL FOR 45000 PSI VALUE.
CAN YOU HELP ME?