Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SAGGING OR BOWING ACCEPTANCE CRITERIA IN FIRED HEATERS?

Status
Not open for further replies.

sappy

Petroleum
Apr 5, 2015
3
1. Please describe the difference between Bowing and Sagging of tubes in Fired heaters and do the same acceptance limits apply for Bowed as well as sagged tubes.
In both sagging and bowing, tubes deformation is due to creep phenomenon as per API RP 573. So the acceptance limit of both sagged or bowed tubes should be same.

As per API RP 573 Edition 2003, TABLE 3 Acceptance limits for tube Deterioration Mechanisms, the acceptance limit for Sagged Tubes is given as 5 * Tube diameter.
Whereas according to ABSA code AB-507 (Edition: 1999, Revision 02) PAGE NO. 8, Tube Bowing acceptance limit is given as 1* Tube diameter.

2. Acceptance limit of Bowing is required in case of vertical tubes of heaters with reference to applicable code and standard.
 