Sale of Company and WPS/PQRs

Status
Not open for further replies.

weeeds

Mechanical
Nov 12, 2003
171
If an ASME fabricator is sold and the new owner has a new name and new physical location, can the new owner also use the WPS/PQRs from the old company if this is included in the purchase agreement?
 
Replies continue below

Recommended for you

The PQR's can be used provided responsibility is accepted and is described in the organizations's quality manual. New WPS's must be written under the new company name. Please review ASME Section IX for details.
 
The WPSs and supporting PQRs are intellectual property. They are transferred to the new owner. As mentioned by others, you need to review ASME Section IX.

Best regards - Al
 
Thank you all very much. This is great information.
 