Wastewatereng
Mechanical
Does anyone have any experience using scotchkote coating for wastewater applications? I have been adviced by a manufacturer that scotchkote tends to break down easily in wastewater, however all the other sites so far have suggested that Scotchkote is Recommended for wastewate uses. So I am really confused as to which to believe. Can anyone offer any help / advance based on past experience?