Oct 20, 2021 #1 EslamSH Materials Oct 20, 2021 8 EG Could you please tell me what tests required for severe sour services? 1- Hardness test 2- SSC 3- HIC 4- All of above tests
Could you please tell me what tests required for severe sour services? 1- Hardness test 2- SSC 3- HIC 4- All of above tests
Oct 20, 2021 #2 EdStainless Materials May 20, 2004 15,893 Waukesha WI USA What kind of application? What MoC? How severe? (there are defined classes) Which Codes are you working to? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
What kind of application? What MoC? How severe? (there are defined classes) Which Codes are you working to? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Oct 20, 2021 #3 SJones Petroleum Apr 22, 2001 3,891 GB Study ISO 15156 Parts 1, 2, and 3, and then come back and ask what you need help with following. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
Study ISO 15156 Parts 1, 2, and 3, and then come back and ask what you need help with following. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer.