Does anyone know what the shear modulus of elasticity of masonry would be, or where i can find that information?

Thanks,

PAT2
 
Replies continue below

Recommended for you

pat2,
Check out ACI 530-02 section 1.8. Shear modulus can be taken as .4Em. Em = 700 f'm for clay masonry, and 900 f'm for concrete masonry.
 