If I have anchor bolts embedded in a CMU wall (f'm=1500psi)that is fully grouted (grout f'c=4000psi), is it ok to use the shear strength values from 1997 UBC Table 19-D for bolts embedded in concrete, rather than the values listed in Table 21-E for bolts embedded in masonry? Or do the values for masonry already take into account fully grouted units with higher strength grout?