Oct 10, 2014 #1 EngMan40 Civil/Environmental Jan 11, 2009 65 0 0 US If anyone can help me put together a checklist for shop welding inspection for built-up columns composed of thick (~4") plates. I know one important aspect of it which is preheat temperature, any suggestions?