terry8u8
Materials
- Feb 27, 2009
- 8
Do 508×42, material is 15NiCuMoNb5, PO standard is EN 10216-2
In the mandatory test section of table 13 of EN 10216-2 , it says that “Flattening test for D < 600 mm and T/D ratio ? 0,15 but T ? 40 mm or Ring tensile test for D > 150 mm and T ? 40 mm”
I don’t catch the meaning of the word “but “ , I think pipe whose wall thickness more than 40mm has no need for Flattening test. Because the wall thickness is too high to do Flattening test But these tests are mandatory. I am confused
In the mandatory test section of table 13 of EN 10216-2 , it says that “Flattening test for D < 600 mm and T/D ratio ? 0,15 but T ? 40 mm or Ring tensile test for D > 150 mm and T ? 40 mm”
I don’t catch the meaning of the word “but “ , I think pipe whose wall thickness more than 40mm has no need for Flattening test. Because the wall thickness is too high to do Flattening test But these tests are mandatory. I am confused