Contech2011
Civil/Environmental
Hi All,
We have a situation where early shrinkage cracks occured after 1-2 hours of the concrete was placed. Enclosed are the pics of these cracks. The grade of concrete is 45 Mpa (flow upto 600mm) and was pumped up 16 storeys by placing boom. Ambient temp was 41 deg centigrade max.. concrete temp 30 degrees max...Observations on-site revealed that no immediate protection was in place by burlaps, PVC sheets, no wind barrication. The surface seemed dry but the concrete was wet inside...The contractor is complaining that the concrete did not set within first 2-3 hours and thats the reason he could not make late finishing and early curing, as the masons feet were inserted into the concrete..
Please analyse the reasons and solutions to avoid such cracks..
We have a situation where early shrinkage cracks occured after 1-2 hours of the concrete was placed. Enclosed are the pics of these cracks. The grade of concrete is 45 Mpa (flow upto 600mm) and was pumped up 16 storeys by placing boom. Ambient temp was 41 deg centigrade max.. concrete temp 30 degrees max...Observations on-site revealed that no immediate protection was in place by burlaps, PVC sheets, no wind barrication. The surface seemed dry but the concrete was wet inside...The contractor is complaining that the concrete did not set within first 2-3 hours and thats the reason he could not make late finishing and early curing, as the masons feet were inserted into the concrete..
Please analyse the reasons and solutions to avoid such cracks..