Colleagues:
Has anyone had to deal with the common mis-installation of Simpson (or equivalent)anchor straps and their incorrect attachment to the mudsill? (i.e., not spreading the straps to the "Y" position prior to embedment, and if spreading is not, done, the carpenters do not drill holes through the mudsill and wrap the straps out, but rather just wrap the straps around the mudsill, creating a "spring" condition.)
What are the possible problems that can arise from this mis-installation?
Are the building inspectors responsible for checking this critical detail? What action may (should) they take if they see this incorrect installation?
Corollary Question:
What is the minimum thickness of CMU block that can be used atop a trench footing as an extension of that footing for the attachment of a mudsill and wall? (i.e., a typical garage foundation detail.) Does the CMU block need to be mechancally attached to the trench footing with vertical rebar in grouted cells? Can solid CMU units be used? Has anyone seen the straps installed in the headjoints?
(Code reference: BOCA)
regards
Has anyone had to deal with the common mis-installation of Simpson (or equivalent)anchor straps and their incorrect attachment to the mudsill? (i.e., not spreading the straps to the "Y" position prior to embedment, and if spreading is not, done, the carpenters do not drill holes through the mudsill and wrap the straps out, but rather just wrap the straps around the mudsill, creating a "spring" condition.)
What are the possible problems that can arise from this mis-installation?
Are the building inspectors responsible for checking this critical detail? What action may (should) they take if they see this incorrect installation?
Corollary Question:
What is the minimum thickness of CMU block that can be used atop a trench footing as an extension of that footing for the attachment of a mudsill and wall? (i.e., a typical garage foundation detail.) Does the CMU block need to be mechancally attached to the trench footing with vertical rebar in grouted cells? Can solid CMU units be used? Has anyone seen the straps installed in the headjoints?
(Code reference: BOCA)
regards