Sodium Hypochlorite Injection pumps for offshore platform

Status
Not open for further replies.

vjr0512

Mechanical
Jun 6, 2011
114
As per NORSOK standard, i have to use either Titanium or GRP for the above process liquid. But for the Injection pumps ( Positive Displacement , Diaphragm pumps), Titanium Head for the pumps are highly costly. Thanks to suggest acceptable alternative which i can suggest to the client.
 
Replies continue below

Recommended for you

What is the concentration of Sodium Hypochlorite? There are stainless steels which are resistant against Sodium Hypochlorite - depending upon concentration and temperature.
 