Jul 9, 2009 #1 msmamma Materials Jul 9, 2009 1 US I am trying to come up with a transparent medium in which to incorporate scatters and dye and make a solid phantom. I cannot find an epoxy to use that is optically clear nor a standard that can be removed from a mold. Any suggestions?
I am trying to come up with a transparent medium in which to incorporate scatters and dye and make a solid phantom. I cannot find an epoxy to use that is optically clear nor a standard that can be removed from a mold. Any suggestions?
Jul 9, 2009 #2 IRstuff Aerospace Jun 3, 2002 44,378 US Don't people normal use acryllic for this? TTFN FAQ731-376 Upvote 0 Downvote
Jul 9, 2009 #3 patprimmer New member Nov 1, 2002 13,816 US Yes they do. Acryic casting resins also known as methyl methacrylate casting resins. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
Yes they do. Acryic casting resins also known as methyl methacrylate casting resins. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules
Jul 10, 2009 #4 lumenharold Mechanical Sep 6, 2006 305 US A quick search turned up these sites athough a couple of the documents are not free: http://adsabs.harvard.edu/abs/1988PhDT........82H http://www.iop.org/EJ/abstract/0031-9155/42/10/011 http://www.warf.org/ipstatus/P95006US.PDF Harold SW2009 SP2.0 OPW2009 SP0 Win XP Pro 2002 SP3 Dell 690, Xeon 5160 @3.00GHz, 3.25GB RAM nVidia Quadro FX4600 http://www.lumenflow.com Upvote 0 Downvote
A quick search turned up these sites athough a couple of the documents are not free: http://adsabs.harvard.edu/abs/1988PhDT........82H http://www.iop.org/EJ/abstract/0031-9155/42/10/011 http://www.warf.org/ipstatus/P95006US.PDF Harold SW2009 SP2.0 OPW2009 SP0 Win XP Pro 2002 SP3 Dell 690, Xeon 5160 @3.00GHz, 3.25GB RAM nVidia Quadro FX4600 http://www.lumenflow.com