Solution annealing of U-bend Tp304 tubes

Status
Not open for further replies.

teokal

Mechanical
May 4, 2007
77
Hi all,
is solution annealing required for seamless Tp304 H/E tubes 3/4" and 1" after U-bending?
Or any other heat treatment?
thank you
 
Replies continue below

Recommended for you

What is the material specification? For this type of bend radius, I would solution anneal to assure maximum corrosion resistance.
 
The material spec is SA213 Tp304 (UNS S 30400), 3/4" and 1" are the tubes' outside diameters and the U-bend radius will be minimum 35mm; maximum U-bend radius will be approx. 120mm.
 
Not required by code, but good practice.
 