Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Specific Heat Capacity Ranges for La and Ce

Status
Not open for further replies.

dcopps

Mechanical
Feb 8, 2005
70
I am seeking variations in the constant-pressure specific heat capacity up to the boiling point for Lanthanum (La) and Cerium (Ce). I understand this value varies a good bit with temperature, so am looking for a plot of some kind.
 
Replies continue below

Recommended for you

Hi

Well these data are from Perry's handbook. Unfortunatly they don't go pretty much in the near of the boiling point.

la(273–1009)

CP=5.91 + 0.00100T cal/(molK)

Ce (273K–908K)

CP=5.88 + 0.00123T cal/(molK)

 