Jun 13, 2006 #2 swall Materials Sep 30, 2003 2,764 Yes, 1144 can be spheroidized. But, if you are hoping that this will increase some formabililty parameter, you may be out of luck, as the sulfur inclusions will then be the limiting factor for formability. Upvote 0 Downvote
Yes, 1144 can be spheroidized. But, if you are hoping that this will increase some formabililty parameter, you may be out of luck, as the sulfur inclusions will then be the limiting factor for formability.
Jun 13, 2006 #3 TVP Materials Apr 12, 2002 4,592 As swall said, 1144 steel can be spheroidize annealed. Upvote 0 Downvote