Hello.
We have a 300PSIG MAWP - 20700lb/hr natural gas powered boiler. We have had three different spiral gaskets unwind shortly after startup. Two of them are installed by one tech and the third by different tech. The first one started leaking right off the bat where as the second one unwound but did not leak for several weeks. The third one was installed yesterday and unwound shortly after startup. It is the gasket for the man hole cover. The cover is held in place with two studs and it is an oval shaped gasket.
Could we have perhaps gotten a bad batch of gaskets? Since it's two different techs that installed them and it's only two studs to tighten, I don't believe installation is the issue. I'm not 100% sure as I have not seen them put them in. We have a contractor do our boiler work. Should I ask to use a solid graphite gasket instead?
We have a 300PSIG MAWP - 20700lb/hr natural gas powered boiler. We have had three different spiral gaskets unwind shortly after startup. Two of them are installed by one tech and the third by different tech. The first one started leaking right off the bat where as the second one unwound but did not leak for several weeks. The third one was installed yesterday and unwound shortly after startup. It is the gasket for the man hole cover. The cover is held in place with two studs and it is an oval shaped gasket.
Could we have perhaps gotten a bad batch of gaskets? Since it's two different techs that installed them and it's only two studs to tighten, I don't believe installation is the issue. I'm not 100% sure as I have not seen them put them in. We have a contractor do our boiler work. Should I ask to use a solid graphite gasket instead?