is spwht required by section VIII for 9cr material and if so is impacts required to be done after spwht is performed on the sample.
 
Replies continue below

Recommended for you

PVF, there is a lot you've not said (like exactly what you mean by 9 Cc) but I'd say 1) yes per UCS-85 and 2) yes per UG-84(f)(2).