Hello Guys,
Please let me know if shape factor and shear stifness calculation below is correct for attached rubber design.
Thank you.
A=Load area
B=Bulged area
D=Outside dia.
d=inside dia.
L=Thickness of rubber
t=Undeformed thickness
k=dynamic shear stiffness
G=dynamic shear modulus
A= pi*(D+d)*L
B= pi*D*L
SF= A/B
t= (D-d)/2
k= A*G/t