Could you supply more information about the designation? 319-T51 would refer to a permanent mold 319 alloy casting that is artificially aged (i.e. no solution treatment). But the SR prefix is one that is not known to me.
 
The "SR" could indicate a strontium modified casting. Addition of small amounts of strontium causes the hypoeutectic silicon particles to become much finer than in a non-modified casting and this will increase mechanical properties somewhat.
 