I have a vessel in cold service (SA-240 Gr316L) and am wondering what structural stainless steel is commonly used for supports?
 
Replies continue below

Recommended for you

We generally use 304/304L for externals, even on 316 vessel
 
SA240 is a standard applicable to plate whereas SA276 is a standard applicable to bars and structural shapes.

You could use SA240 to order plate to fabricate structural members but if you wanted to order structural shapes (angle iron, channels, etc.) SA276 would be the appropriate standard.
 
if what we need is not available in structural shapes .... we will fabricate from plate sa-240
 