JTHawkins

Specifier/Regulator
Apr 28, 2011
3
Hello to all.
I am in the freight and transit railroad industry as a Welding Mfg. Engineer/CWI. I am currently qualifying welding procedures and am having to deal with several AISI steels. Is there a way that the AISI numbers can be cross referenced to an ASTM standard? I am trying to group my material to cut down on the number of qualifications and total costing.



Thanks for the input!
 
Replies continue below

Recommended for you

Check out for equivalent numbers to different specs.

"Wildfires are dangerous, hard to control, and economically catastrophic."

Ben Loosli
 
@ looslib

Thanks, I have looked at this website many times and it has proven to be helpful. There are several materials that I need a cross reference on and they are not listed on Matweb.

Thank you for the reply
 
I would suggest you purchase the following document for your use;

AWS B2.1 Specification for Welding Procedure and Performance
Qualification

There is a Table D that provides base metal grouping for welding. Each metal is listed by Grade, Type, etc with corresponding ASTM specification number followed by an AWS M-No grouping number for welding.
 
I have the latest edition of B2.1. That is what I am qualifying to, but the materials in question are "unlisted" My qualifications will be for 22 separate base metal combinations. These combinations are made up of pre-qualified, listed, and unlisted materials. The AISI steels in question are all carbon steel, but do not show up in Table D of B2.1 For instance, AISI 1541 and AISI 1040. These are just two of the AISI steels I am dealing with. With that being said, should I assume that all AISI steels would conform to ASTM A830 / A830M - 02 Standard Specification for Plates, Carbon Steel, Structural Quality, Furnished to Chemical Composition Requirements?
 
With that being said, should I assume that all AISI steels would conform to ASTM A830 / A830M - 02 Standard Specification for Plates, Carbon Steel, Structural Quality, Furnished to Chemical Composition Requirements?

For purposes of weld qualification, yes.
 