We are trying to source some 4340 steel to AMS-S-5000 or AMS 6359, box section (RHS) approximately 30mm x 30mm x
3mm thick. Also the same steel in 3mm and 5mm plate as well as 40mm x 3mm equal angle. Any suggestions?
 
Replies continue below

Recommended for you

I have used Atlas Speciality Steel, Welland Ont. for this grade, not sure of their size/shape capabilities.

Also, you may want to try Universal Stainless and Alloy, Brdigeville, PA.
 