We are looking for a non-destructive method to determine the thickness of a stellite weld overlay on tubing. Does anyone have any experience with this?
 
Replies continue below

Recommended for you

Is the material in the as welded condition or has it been machined?
If the tube diameter is known why not a physical measurement?
 
Overlay has been welded. We thought about diameter measurements, but the tube diameter won't always be accurately known.
 
Did you investigate ultrasonic testing techniques?
 
I don't know how thick the stellite is, I would recommend using a Mil Tester.

Petrotrim Services
 