I have a situation where I need to support a 6" stone veneer over an arched opening. we want the stone to "wrap" under the arch (ie no exposed steel lintel) Its a very flat arch. Nothing at each end to support the thrust of a true arch. Is there any concealed system out there to support natural stone in this condition?
 
Replies continue below

Recommended for you

I have used cast-in-place concrete with a brick veneer arch/soffit. You line the falsework with brick that have anchors to engage the conrete. Once the beam is cast and the forms removed all you see is brick. You will need a method of anchoring the stone into the concrete, but there may be a method out there.
 