How does one determine a resonable strenght and modulus for old timber in the order of 50 to 100 years old?
 
Replies continue below

Recommended for you

What type of wood is it and where is it located?
 
To Kramer: This is a general question applicable to various species and locations.
 
check with the u.s. forest service lab in madison, wis. they are the wizard in wood research and testing. ansel
 