strength vs temperaure of 4310? 3

Status
Not open for further replies.

salmon2

Materials
Feb 1, 2008
360
Can anyone please point me at some websites I can find the strengh/temperature dependency of 4130 chemistry? I am not sure about the heat treatment condition yet, could be normalized or Q&Ted. But just wonder if any websites I can find some related data. Thanks a lot.
 
Replies continue below

Recommended for you

There is an ASM High Temperature Properties of Ferrous Metals handbook. It has very detailed and accurate information.

= = = = = = = = = = = = = = = = = = = =