Sep 28, 2011 1 #2 SnTMan Mechanical Jan 22, 2005 6,794 Sec I, Sec III, not permitted, Sec VIII, Div 1, Sec XII, 21400 psi Regards, Mike Upvote 0 Downvote
Sep 28, 2011 Thread starter #3 qcrobert Industrial Jun 24, 2010 229 Thank you SnTMan, for your quick response and additional information! Upvote 0 Downvote