We have a project where we are looking to use bronze as the structural support elements. Does anyone know of any design information regarding bronze? We would also be happy with finding any projects or designers that have used structural bronze and talking to them to get some technical insight. I have done some googling and have not found much but hoping the group here might have some other leads.