I have spec'd 16" O.D. round HSS for a project (bending application). The fabricator has a large quantity of 16" O.D. API 5L X70 that is available at less cost. The yield strength of the API pipe is greater but I'm not familiar with the API standards. Is anyone familiar with API and its use in a structural application?